[1]郭登明,周靖力,肖信武,等.延長高壓活動彎頭壽命的工藝研究[J].石油機械,2017,45(05):86-88,94.[doi:10.16082/j.cnki.issn.1001-4578.2017.05.016]
 Guo Dengming,Zhou Jingli,Xiao Xinwu,et al.Study on the Technology for Extending Service Life of High Pressure Movable Elbow[J].China Petroleum Machinery,2017,45(05):86-88,94.[doi:10.16082/j.cnki.issn.1001-4578.2017.05.016]
點擊復制

延長高壓活動彎頭壽命的工藝研究

參考文獻/References:

[1] 龔桂仙,韓榮東,孫宜強.壓裂車活動彎頭爆裂分析[J].武鋼技術,2011,49(3):30-33.
[2] 徐曉東,黃志國.提高高壓活動彎頭體使用壽命的工藝途徑[J].機械設計與制造,2005(8):118-119.
[3] 張繼信,樊建春,張來斌,等.30CrMo合金鋼的沖蝕磨損性能研究[J].潤滑與密封,2012,37(4):15-18.
[4] ZHOU X X,LEA C J.Three-demensional computional fluid dynamic modeling of natural gas releases from high pressure pipelines[C].Pipe & Pipelines International,1997(9/10):13-24.
[5] 謝永金,樊建春,張宏,等.頁巖氣開發用高壓管匯損傷機理及檢測技術[J].石油機械,2011,39(增刊1):109-112.
[6] 劉春城.高壓管匯破損預測技術研究[D].大連:大連理工大學,2000.
[7] 丁小軍,李福泉,寵小軍,等.高壓管匯的在役檢測[J].無損檢測,2010,32(4):306-308.
[8] 喻建勝.高壓管匯螺紋部位的超聲相控陣檢測應用研究[J].鉆采工藝,2016,39(3):80-82.
[9] 李鳳照,姜江,張正中,等.貝氏體鋼的顯微組織和耐磨性[J].金屬熱處理,1994(4):11-15.
[10] 王洪發,夏放.貝氏體鋼抗磨料磨損性能的研究[J].鋼鐵,1984,19(10):36-41.
[11] 王志奮,吳立新,劉敏,等.貝氏體鋼的耐腐蝕性能研究[J].武漢工程職業技術學院學報,2013,25(2):15-18.

相似文獻/References:

[1]朱中平,黃朝斌,喬春,等.SJX5270TYG壓裂管匯車的研制[J].石油機械,2011,(02):69.
[2]張繼信,樊建春,李世玉,等.高壓管匯的檢測及安全評價技術研究[J].石油機械,2012,(01):64.
[3]符方杰,樊建春,張繼信.腐蝕缺陷對高壓管匯剩余強度的影響分析[J].石油機械,2012,(06):66.
[4]吳漢川,王峻喬,余旭陽. 大型壓裂施工裝備的配置與連接[J].石油機械,2014,(04):67.
 [J].China Petroleum Machinery,2014,(05):67.
[5]孫秉才,樊建春,溫東,等. 高壓管匯沖蝕磨損磁記憶檢測試驗研究[J].石油機械,2014,(06):65.
 [J].China Petroleum Machinery,2014,(05):65.
[6]潘靈永,王峻喬,周斌,等.基于CFD技術的高壓管匯系統布局優化設計[J].石油機械,2016,44(07):94.[doi:10.16082/j.cnki.issn.1001-4578.2016.07.020]
 Pan Lingyong,Wang Junqiao,Zhou Bin,et al.CFD-based Optimum Design for High Pressure Manifold Layout[J].China Petroleum Machinery,2016,44(05):94.[doi:10.16082/j.cnki.issn.1001-4578.2016.07.020]
[7]孫汝奇,岳愛麗,劉忠硯,等.高壓作業下管匯的空間流固耦合分析[J].石油機械,2016,44(07):103.[doi:10.16082/j.cnki.issn.1001-4578.2016.07.022]
 Sun Ruqi,Yue Aili,Liu Zhongyan,et al.Spatial Fluid-solid Interaction Analysis of Manifold in High Pressure Operation[J].China Petroleum Machinery,2016,44(05):103.[doi:10.16082/j.cnki.issn.1001-4578.2016.07.022]
[8]涂亞東,徐小兵,殷華鋒,等.高壓管匯沖蝕磨損規律研究[J].石油機械,2018,46(02):84.[doi:10.16082/j.cnki.issn.1001-4578.2018.02.015]
 Tu Yadong,Xu Xiaobing,Yin Huafeng,et al.Analysis on Erosion Wear Laws of High Pressure Manifold[J].China Petroleum Machinery,2018,46(05):84.[doi:10.16082/j.cnki.issn.1001-4578.2018.02.015]
[9]郭登明,吳海鋒,郭建東,等.用于超高壓管匯材料15CrNiMo的綜合性能研究[J].石油機械,2019,47(04):104.[doi:10.16082/j.cnki.issn.1001-4578.2019.04.017]
 Guo Dengming,Wu Haifeng,Guo Jiandong,et al.Comprehensive Performance Study of 15CrNiMo for Ultra-high Pressure Manifold Material[J].China Petroleum Machinery,2019,47(05):104.[doi:10.16082/j.cnki.issn.1001-4578.2019.04.017]
[10]李方淼,李美求,宋楊,等.液固兩相流對活動彎頭的沖蝕研究[J].石油機械,2019,47(10):107.[doi:10.16082/j.cnki.issn.1001-4578.2019.10.018]
 Li Fangmiao,Li Meiqiu,Song Yang,et al.Erosion of Liquid-Solid Two-Phase Flow on Bend Pipe Union[J].China Petroleum Machinery,2019,47(05):107.[doi:10.16082/j.cnki.issn.1001-4578.2019.10.018]
[11]郭登明,汪隨,卞和滿.高壓管匯活動彎頭的接觸分析及結構改進[J].石油機械,2018,46(03):72.[doi:10.16082/j.cnki.issn.1001-4578.2018.03.013]
 Guo Dengming,Wang Sui,Bian Heman.Contact Analysis and Structural Improvement of the Swivel Joints in High Pressure Manifold[J].China Petroleum Machinery,2018,46(05):72.[doi:10.16082/j.cnki.issn.1001-4578.2018.03.013]

備注/Memo

收稿日期:2016-12-23。
作者簡介:郭登明,教授,生于1963年,1985年畢業于江漢石油學院機械工程系,現從事石油機械的教學、科研與設計工作。地址:(434023)湖北省荊州市。E-mail:[email protected]